COMPOSITE FILM OF PRE-COATING TECHNOLOGY
Simplified Process:
Eliminates the need for paint coating process.
Capable of producing a diverse range of colorful flooring options.
High Performance Composite Film + Three-Dimensional Textures, Breaking the Boundaries of Traditional Membrane Materials
CPCT film represents Composite PVC Film of Pre-Coating technology. A specialized UV coating is applied to the surface of the PVC film, imparting functionalities such as anti-scratch, stain resistance, and antimicrobial properties. This treated PVC film is then laminated to various printed decorative membranes using a high-temperature lamination machine, while simultaneously undergoing embossing via an embossing roller to yield the CPCT film. A variety of textures can be offered according to market demand, including straight-line patterns, marble patterns, woodgrain, and frosted finishes, among others.
Applications:
Utilizing PUR adhesive lamination technology, primarily intended for surface finishing of flat panels like furniture composites, inorganic boards, and medium-density fiberboards, with a PUR glue application rate of 60-90 g/m².
Exceptional Performance Crafting A+ Home Membrane Materials
Key Highlights:
ØHigh Efficiency, Low Production & Installation Costs: Achieves high productivity, with the capability to produce 3,000 to 4,000 m² of finished product within an 8-hour shift, requiring minimal labor.
ØSuperior Quality: Free from issues such as gloss spots, roller marks, color disparities, or odors.
ØHigh Adaptability: Offers multiple functional choices, e. g., stain resistance, scratch resistance, high wear resistance, antimicrobial properties, etc.
Performance Test:
Test items |
Testing standards |
Testing unit |
Detection value |
|
Wear resistance of the surface |
Abrasion resistance |
EN 13329(S42) |
r |
≥2000r |
Wear value |
GB/T 17657-2013 |
g/100r |
≤0.08g/100r |
|
Adhesion |
ASTM D3359 |
B |
5B |
|
Hardness |
ASTM D3363 |
H |
≥2H |
|
Scratch resistance |
EN 438-2 |
N |
2N |
|
Micro-scratch resistance |
EN 16094 |
Class |
MSR-B2 |
|
Immersion peel test |
GB/T 18103-2013(73℃2h,63℃3h) |
mm |
No delamination |
|
Drop ball impact test |
GB/T 17657-2013 |
mm |
No cracks,10mm |
|
Chemical corrosion resistance |
ASTM F3261(5%NaOH,16h) |
/ |
No corrosion |
|
Contamination resistance |
GB/T 17657-2013(soy sauce, vinegar, and olive oil,24h) |
/ |
No contamination |
|
Cold and hot temperature cycling |
GB/T 17657-2013(80℃2h,-20℃2h,four cycles) |
mm |
No cracks |